1. Product Introduction
Having sufficient mixing time for highly active stone materials, it can produce mixed emulsified asphalt such as BC-1, BCR, etc.
2. Instructions for use
It can be pumped above 20 ℃, and when in use, it can be added to hot water and stirred until completely dissolved. The pH value can be adjusted to 2.0-3.0 with industrial acidic substances, and it can be used for emulsified asphalt production.
3. Applicable process
Slurry sealing layer, micro surface area.
4. Technical indicators
Appearance: Black brown viscous liquid
Active ingredient content: 52 ± 2%
PH value: 8-10
Dosage: 1.8% -2.2% (short-term storage) 2.0% -2.5% (long-term storage)
Packaging: 200kg/drum