1. Product Introduction
The active ingredient content can reach up to 70%, and there is sufficient mixing time for highly active stone materials in high temperature environments to produce blended emulsified asphalt, such as: BCR-A、BCR-B、 Cold regeneration, etc.
2. Instructions for use
It can be pumped at temperatures above 20 ° C. When in use, it can be added to hot water and stirred until completely dissolved. By adjusting the pH value to 2.0-3.0 with industrial acidic substances, it can be used for emulsified asphalt production.
3. Applicable process
Slurry sealing layer, micro surface area.
4. Technical indicators
(1) Appearance: Red viscous liquid
(2) Active ingredient content: 70 ± 2%
(3) PH value: 8-10
(4) Dosage: 1.8% -2.2% (short-term storage) 2.0% -2.5% (long-term storage)
(5) Packaging: 200kg/drum